模具收缩率,流动,3.2毫米。
采用一般的平均收缩率方法来确定模具型腔的成型尺寸,已难以满足精密注塑成型制品的精度要求。
Using average shrinkage rates of injection-molded parts to decide the dimension of mold cavity can not satisfy the demand of high precision injection-molded parts.
本文主要研究了固化剂、纳米二氧化硅粉和碳酸钙粉等外加剂对硅橡胶模具线收缩率的影响。
The effects of solidified agent, nanometer silicon dioxide powder and calcium carbonate powder on line contraction percentage of silicon rubber mould were discussed in this paper.
塑料的成型收缩率直接关系到制品的形状和尺寸精度,因此在塑料注射成型的模具设计中,迫切需要预测制品的成型收缩率。
The shrinkage of plastic products is a very important parameter and need to be forecast during the design of injection molds, which affects the shape and size precision of the products.
并就简化模具结构设计的优缺点与前后三次激光选区烧结(SLS)的成型工艺条件和收缩率进行了探讨,提出了SLS技术的现状、发展趋势与方向。
The advantages and disadvantages of simplifying the mould structure, and the molding condition and contraction rate of the successive SLS three times are discussed.
公司产品品种达几十种,为你的模具制作提供快速的复制,精密的收缩率,产品的收缩率可以达到千分之二。
With a product line of tens of categories, we can offer quick copying with precise contraction ratio (up to two thousandth) for mold making.
材料置于模具中进行干燥可以消除水平方向的收缩,但高度方向的收缩率大于无模具干燥下的收缩率。
Drying the materials in a restricting mold diminished the horizontal shrinkage, and the vertical shrinkage was higher than that in the mold-less drying.
运用该方法设计出一套测试模具,通过该模具就完全掌握了该合金的真实收缩率。
Using the method, a set of testing die was designed, and the real contractive rate of alloy was known by the die.
运用该方法设计出一套测试模具,通过该模具就完全掌握了该合金的真实收缩率。
Using the method, a set of testing die was designed, and the real contractive rate of alloy was known by the die.