The effect of normalizing on microstructure, strength, impact toughness and ductile-brittle transition temperature of FAS390Q axle housing steel was studied.
研究了正火处理对FAS390Q桥壳钢显微组织、强度、冲击韧性和韧脆转变温度的影响。
The main effect of water on brittle plastic transition of mafic rocks is embodied by both the change of strength and temperature of brittle ductile transition and brittle plastic transition.
水对基性岩脆塑性转化的影响体现在岩石的强度和脆延性与脆塑性的转化温度两方面。
High manganese steels undergo a ductile to brittle transition at low temperature, which is accompanied by a change in the fracture mechanism from dimple fracture to intergranular fracture.
高锰奥氏体钢随温度降低其断裂机制由韧窝状断裂转变到晶界断裂。
The specimens with Widmanstatten structure have higher impact strength and lower ductile-brittle transition temperature than those with equiaxial granular ferrite structure.
有魏氏组织的试样较呈等轴铁素体的试样有更高的冲击韧性和更低的韧脆转变温度。
The specimens with Widmanstatten structure have higher impact strength and lower ductile-brittle transition temperature than those with equiaxial granular ferrite structure.
有魏氏组织的试样较呈等轴铁素体的试样有更高的冲击韧性和更低的韧脆转变温度。