Chemical passivation: will contain antioxidant parts in solution in processing, make the surface to form a thin film of the state of the process. Blunt.
化学钝化:将制件放在含有氧化剂的溶液中处理,使表面形成一层很薄的钝态保护膜的过程。
A novel passivation technology of porous silicon (PS) surface, i. e. , depositing diamond film on the PS surface by microwave plasma assisted chemical vapor deposition (MPCVD) method, was developed.
提出了一种新颖的多孔硅表面钝化技术,即采用微波等离子体辅助的化学气相沉积(MPCVD)方法在多孔硅上沉积金刚石薄膜。
Several alternative chemical treatments are defined for passivation of stainless steel parts.
几种可供选择的不锈钢部件化学钝化处理在此有详细规定。
Unless specified by the purchaser, the chemical treatment applied to the stainless steel parts shall be selected by the seller from among the listed passivation treatments.
除非买方指定,应用到不锈钢部件的化学处理应由卖方从列出的钝化处理中选定。
The article introduces the post-disposal technology of chemical washing and also discusses the fulling and passivation processes.
介绍了进行化学清洗的后处理技术,并对漂洗和钝化工艺进行了讨论。
The Company are to develop and produce specialized cleaning, rust removal, passivation, water treatment agents and other related chemical products chemical companies.
本公司是专门研制生产清洗、除锈除油、钝化、水处理剂及其它相关化工产品的化工企业。
Passivation is a method by which chemical agents react with metal surfaces to render the surfaces nonreactive.
钝化是由化学试剂与金属表面产生反应给与表面不反应的方法。
An environmentally-friendly chemical polishing and passivation process was established for copper and its alloys, using a rare earth salt in the passivation solution.
为了提高铜及其合金的表面抗变色能力,研制了一种环保的化学抛光工艺和含稀土盐的新型钝化工艺。
The passivation process defined in 3.1.1.2 will occur without further chemical treatment, but may be augmented and improved by the post-cleaning treatments defined in 3.1.1.3.
钝化过程(在3.1.1.2说明)在没有进一步的化学处理情况下也会发生,但钝化作用将会被“后清洗处理”(在3.1.1.3说明)提高增强。
Should be strict control in the passivation process of chlorine ion in the passivation solution, the passivation with chemical material used for chloride ions are limited.
在钝化历程中应严酷控制钝化液中氯离子含量,所用钝化用化学质料对氯离子都有限量要求。
The new sulfur passivation technique developed in late 80's injects new life into the study of the passivation although the chemical stability of the passivation layer is not so satisfactory.
八十年代后期出现的硫钝化技术给钝化研究注入了活力,但它的化学稳定性仍不够理想。
The new sulfur passivation technique developed in late 80's injects new life into the study of the passivation although the chemical stability of the passivation layer is not so satisfactory.
八十年代后期出现的硫钝化技术给钝化研究注入了活力,但它的化学稳定性仍不够理想。
应用推荐