The local cleavage fracture stress is mainly determined by the length of the critical microcrack.
细观解理断裂应力主要由临界裂纹的长度决定。
Dimensions of the stress and crystalline have influence on cleavage fracture.
应力的大小和晶粒的尺寸影响解理断裂。
Scanning electron microscopy analysis on blade fracture shows: the fracture is characterized by cleavage, quasi-cleavage and stress corrosion and so on.
对叶片断口扫描电镜分析显示,断口具有准解理、韧窝、应力腐蚀等复杂特征。
The stress corrosion cracking sensitivity of the steel was low, and the fractography of its stress corrosion cracking showed transgranular and quasi-cleavage fracture with secondary cracks.
研究表明该钢具有较好的抗应力腐蚀性能,其应力腐蚀断裂形貌为穿晶、解理断裂,并有二次裂纹。
The cleavage fracture of the notched specimens with various sizes and widths is mainly controlled by the criterion of normal stress.
不同尺寸和宽度的缺口试样的解理断裂主要由正应力判据控制。
The cleavage fracture of the notched specimens with various sizes and widths is mainly controlled by the criterion of normal stress.
不同尺寸和宽度的缺口试样的解理断裂主要由正应力判据控制。