For some applications, especially where extremely high-speed cutting is important, other tool materials such as sintered carbide products are a more economical alternative to tool steel.
对一些应用来说,尤其是非常高速的切削很重要的场合,其它的工具材料比如硬质合金产品是比工具钢更经济的选择。
In many cases of stainless steel cutting operations with carbide tools, a tool life strongly depends on flank notch wear of depth of cut rather than average flank wear of main cutting edge.
硬质合金刀具在不锈钢加工中,其刀具耐用度主要是取决于后刀面边界磨损而不是主切削刃后刀面的平均磨损量。
The mechanism of cutting force, cutting temperature and tool wear in the machining of quenched steel and nickel based high temperature alloy with ceramic tools are analyzed in the paper.
重点分析了陶瓷刀具在切削淬火钢和镍基高温合金中有关切削力、切削温度、刀具磨损等方面的机理。
The cutting experiments show that in cutting of quenched steel the tool life of this cutter is longer than that of uncoated cutting tool.
将氮化碳涂层刀具应用于干切削领域,通过对淬火钢的干式切削试验,研究氮化碳涂层刀具的切削加工性能。
The author gave us the reasonable selection of tool materials, tool parameters and cutting parameters during turning of hardened steel in order to get the ideal cutting result.
着重说明了车削淬火钢件时,如何通过合理地选用刀具材料、刀具几何参数及切削用量达到理想的切削效果,并提出车削淬火钢件时应注意的若干问题。
When the shank size of a cutting tool is large enough, a more viable technique is to braze the carbide tip to a medium carbon steel shank.
当切削刀具的刀柄足够大时,当切削刀具的刀柄足够大时,可行的技术是在中碳钢刀柄上用铜焊接硬质合金刀尖。在中碳钢刀柄上用铜焊接硬质合金刀尖。
The main reason of ceramic tool Wearing is coming off the hard grain during the dry cutting of steel D60.
硬质相颗粒的脱落是干式高速车铣D60钢时金属陶瓷刀具磨损的主要原因。
A diamond coated cutting tool is disclosed having a either steel or cemented carbide substrate.
公开了一种具有钢或硬质合金衬底的金刚石涂覆的切削工具。
The products have been covered: Pliers, cutting, pipe, wrench, tighten, mud wood, torque, storage, hydraulic, lifting, tool steel and other types of applications.
目前产品已涵盖:钳类、剪切、管道、扳手、紧固、泥木、扭力、仓储、液压、起重、钢结构应用等多个工具种类。
Choice of cutting tool, cooling manner and feed path in high speed milling S-136 hardened stainless tool steel were analyzed, based on a S-136 die production.
结合生产,对s- 136淬硬钢高速铣削工艺的刀具选择、冷却方式、进给路线进行了分析。
The modes of tool damage include plastic deformation on cutting edge of high-speed steel tool and tipping of ceramics tool.
刀具破损的主要形式为高速钢刀具切削刃塑性变形和陶瓷刀具的崩刃。
This article introduced the heat-resistant steel machining characteristic and at present USES in cutting the heat-resistant steel the cutting tool material, the cutting tool geometry parameter choice.
介绍了耐热钢切削加工特点及目前用于切削耐热钢的刀具材料、刀具几何参数的选择。
The results showed that the steel after combined treatment had higher surface hardness and wear resistance, and prolonged the service life of cutting tool.
结果表明,该钢经复合处理后,具有较好的表面硬度和良好的耐磨性,显著地增加了刀具的使用寿命。
Carbide Die: including cold heading steel ball mold, cutting tool material, feed tire, the production quality and stability ball mold, long life, can be comparable imported mold.
硬质合金模具:包氨基酸叶面肥括冷镦钢球模具、切料刀、料胎、所生产钢球模具质量稳定、寿命长、可以和进口蔬菜叶面肥模具相媲美。
Repair, such as high-speed tool steel cutting planer tools, high temperature and punching moulds, stamping tools and cutting knife plate rolling and cutting tools under the mold cutting edge.
修复高速工具钢,如切削冲孔和刨工具,高温冲压工具和模具,剪切刀板轧钢和切削工具下模的切削刃口。
It is very hard to process the mini-slender shaft of the stainless steel using the ordinary machine tool because its lower carbon content, great toughness and bad cutting feature.
不锈钢微型细长轴由于含碳量低,韧性大,切削性能差等特点,使得常规设备的加工难以进行。
FS 33ais suitable for machining free cutting steel, steel up to 60 tons tensile strength in multi-spindle, multi-tool lathes and automatics.
FS33A能加工快削钢及60吨以下的拉力钢材,适用于各种传统车床如多转轴、多刀具与及自动车床等。
The utility model relates to a gas cutting tool, particularly to a steel plate gas cutting tool.
本实用新型涉及气割工具,尤其涉及钢板气割工具。
In this paper, the cutting performance of the cutting tool of coated high speed steel is introduced.
介绍了涂层高速钢刀具的切削性能,并列出了涂层与未涂层高速钢刀具的对比切削数据。
In this paper, the cutting performance of the cutting tool of coated high speed steel is introduced.