In this method, the activation energy is reduced during deaminization and the deaminizating rate and the retention of zeolite crystallinity after deaminization are increased.
该方法大幅度地降低了沸石脱胺过程中的活化能,提高了脱胺速率,提高了脱胺后的沸石结晶保留度。