In connection with Meishan Iron for sorting, the final concentrate grade can reach 53.74%, the operating rate was 64.61%, higher than the selected plants on the separation indexes.
针对选别梅山铁矿,其最终精矿品位可以达到53.74%,作业回收率为64.61%,高于选厂分选指标。
In connection with Meishan Iron for sorting, the final concentrate grade can reach 53.74%, the operating rate was 64.61%, higher than the selected plants on the separation indexes.
针对选别梅山铁矿,其最终精矿品位可以达到53.74%,作业回收率为64.61%,高于选厂分选指标。