The sulphur content of final iron concentrate can be decreased to less than 0.5% by using copper sulfate and sodium fluosilicate as activator of pyrrhotite contained in iron ore.
铁矿石选矿中用硫酸铜和氟硅酸钠活化磁黄铁矿,使最终铁精矿合流量降至0.5%以下。