Adding appropriate additive to the calcium Oxide sintered in the high temperature, and controlling the process of hydration will make the expansion fully exert to the fragmentation of rock.
通过向高温死烧过的氧化钙中加入合适的添加剂,对水化过程进行控制,将膨胀能充分利用到介质破碎中。