• The finite element method (FEM) model was established to predict the temperature field, shell growth and solid fraction of the heavy rail bloom caster.

    采用有限元方法某钢厂钢大方坯连铸机凝固过程温度分布情况、坯壳生长规律凝固进行了模拟研究。

    youdao

  • This paper mainly analyzes the process of bloom casting for heavy rail and internal cracks like central crack and so on in order to solve the internal quality problems.

    对方轨钢系列内部产生中间裂、中心缺陷进行工艺探索研究解决生产过程中出现内部质量问题。

    youdao

  • The key technologies, such as M-EMS, secondary cooling scheme, and dynamic soft reduction, and its application to bloom continuous casting for heavy rail steel were presented.

    简述攀钢大方连铸结晶器电磁搅拌技术冷控制技术凝固末端动态下技术连铸中的应用效果。

    youdao

  • The key technologies, such as M-EMS, secondary cooling scheme, dynamic soft reduction, and its application to bloom continuous casting for heavy rail steel were presented.

    简述攀钢大方连铸结晶器电磁搅拌技术冷控制技术凝固末端动态下技术连铸中的应用效果。

    youdao

  • A bloom continuous Casting machine main cast quality steel and alloy steel, such as heavy rail steel, hard-line steel, spring steel, bearing steel, alloy structural steel, and other key species.

    大方连铸机主要浇铸优质合金钢钢、硬线钢、弹簧钢轴承钢、合金结构钢重点品种。

    youdao

  • A bloom continuous Casting machine main cast quality steel and alloy steel, such as heavy rail steel, hard-line steel, spring steel, bearing steel, alloy structural steel, and other key species.

    大方连铸机主要浇铸优质合金钢钢、硬线钢、弹簧钢轴承钢、合金结构钢重点品种。

    youdao