• The results show that the treatment makes the interlaminar shear strength of the composite increased 17.5% and the linear ablation rate decreased 58.6%.

    得出,方法提高复合材料间剪切强度抗烧蚀性能有效方法,它可使层间剪切强度提高17.5 % ,线烧蚀率减小58.6 % 。

    youdao

  • In the range of incident velocities near to the perforation limit velocity (V50), this mechanism depends on thickness and interlaminar shear strength of composite plate.

    接近穿孔极限速度入射速度(V50)范围内,机制依赖复合材料厚度中间层剪切强度

    youdao

  • In the range of incident velocities near to the perforation limit velocity (V50), this mechanism depends on thickness and interlaminar shear strength of composite plate.

    接近穿孔极限速度入射速度(V50)范围内,机制依赖复合材料厚度中间层剪切强度