The concentration of salt and the relative areas of the large cathode coupled with a small magnesium alloy anode have an important effect on the accelerated galvanic corrosion in salt spray test.
盐雾实验中,盐的浓度、大阴极小阳极的面积比以及阴极材料相对于镁阳极的尺寸是加速镁合金电偶腐蚀的重要因素。
At present, the sacrificial anode materials used for the protection of iron and steel, which are based of aluminum, zinc and magnesium alloy.
目前常用的保护钢铁设备的牺牲阳极材料有铝基合金、锌基合金和镁基合金三大类。
AZ31 magnesium alloy was accelerated as anode coupled with dissimilar alloys. The rimous corrosion products sticked to the surface of magnesium alloy.
镁合金与异种合金偶接后,作为阳极被加速腐蚀,腐蚀产物呈龟裂状附着在镁合金基体表面。
AZ31 magnesium alloy was accelerated as anode coupled with dissimilar alloys. The rimous corrosion products sticked to the surface of magnesium alloy.
镁合金与异种合金偶接后,作为阳极被加速腐蚀,腐蚀产物呈龟裂状附着在镁合金基体表面。