The impact toughness, crack forming energy and crack extension energy of complex modified medium manganese austenitic steel. Are increased by 263%? 288% and 232% respectively.
复合变质中锰奥氏体钢的冲击韧度、裂纹形成功和裂纹扩展功分别比原来提高了263%、288%和232%。