The present invention provides one kind of quickly demolding nylon-66 resin and its preparation process.
本发明提供了一种快速脱模尼龙66树脂及其制备方法。
Toughened, heat stabilized Nylon 66 resin for extrusion.
增韧,热稳定尼龙66树脂挤出。
Nylon 66 was effectively toughened with potassium titanate whiskers which were surface modified with an elastic epoxy resin.
钛酸钾晶须用弹性体表面改性后实现了对尼龙66的有效增韧。
Nylon 66 was effectively toughened with potassium titanate whiskers which were surface modified with an elastic epoxy resin.
钛酸钾晶须用弹性体表面改性后实现了对尼龙66的有效增韧。