The grain size differs obviously with the time of ball milling and it reaches the smallest value when been ball milled for 15~20 hours. The grain size also grows when annealed at certain temperature.
结果表明在行星球磨方法下,球磨15到20小时材料晶粒达到最小,在一定温度下退火之后材料晶粒长大。