The output power is very stable after the temperature cycling and vibration test. No apparent power decrease has been observed as the device working continuously for 500 h.
该光纤耦合模块连续工作500小时没有发现明显的功率衰减,并且输出功率经温度循环和振动冲击后具有较好的稳定性。
The thermal fatigue test was performed on 316 SS to understand the crack propagation behavior underthe cycling temperature environment.
从实用出发对316不锈钢管材进行了热循环下的裂纹扩展试验。
The thermal fatigue test was performed on 316 SS to understand the crack propagation behavior underthe cycling temperature environment.
从实用出发对316不锈钢管材进行了热循环下的裂纹扩展试验。