针对螺旋埋弧焊钢管横向板状试样在拉伸试验时存在的屈服强度误差较大的问题,分析了其误差较大的原因,并提出了相应的解决办法。
To the problem of more yield strength error in SSAW pipe transverse strip specimen tensile tests, analyze the reason of the error, put forward corresponding solving method.
添粉和不添粉的5A02和5A06铝合金拼焊板的横向拉伸试件均断裂于薄板母材,证明焊缝的强度合格。
The longitudinal tension PM specimen of Tailor Welded Blanks of 5A02 and 5A06 were all fractured on the thinner base metal, which indicated that welds were eligibility.
在常响应界面情况下,复合材料横向拉伸应力-应变曲线存在明显的转折点,对应于界面分离的起始点,转折点的位置取决于界面粘结强度。
The stress-strain curve under transverse loading of MMCs has a corner point, associated with the initiation of interfacial de-bonding, which is determined by the interfacial bonding strength.
在常响应界面情况下,复合材料横向拉伸应力-应变曲线存在明显的转折点,对应于界面分离的起始点,转折点的位置取决于界面粘结强度。
The stress-strain curve under transverse loading of MMCs has a corner point, associated with the initiation of interfacial de-bonding, which is determined by the interfacial bonding strength.