By cleaning molten steel, controlling casting temperature and withdrawal speed, the compliance ration in ultrasonic inspection of plate was enhanced from 82.5% to 92%.
采取提高钢质纯净度、控制浇注温度和拉速等改进措施,检测合格率由82.5%提高到92%。