The brittle morphologies become much more notable, and appear the inter-and trans-granular fracture mode after sodium corrosion at high temperature for both of W-specimens.
钠腐蚀后,两种钨试样的沿晶脆断特征变得更为显著,为沿晶和穿晶混合型脆性断裂。