Porosity increases along with the increasing of coagulation bath temperature, and doesn't have relation to pre-evaporation.
孔隙率随着凝固浴温度的上升而上升,而与预蒸发时间的长短没有关系;
The results showed that the properties of the regenerated bamboo fiber prepared with lower coagulation bath temperature were improved.
实验结果表明:在较低的凝固浴温度下纺制得到的再生竹纤维素纤维的性能较好。
The effects of spinning dope concentration, coagulation bath temperature and addition of persimmon leaves on the mechanical properties of blend fiber were studied.
研究了纺丝原液浓度、凝固浴温度、柿叶添加量对共混纤维的力学性能的影响。
The retention rates of Albumin bovine decreases when coagulation bath temperature increases, and first decreases, then increases when pre-evaporation time prolongs.
对牛血清白蛋白的截留率随着凝固浴温度的上升而下降,随着预蒸发时间的延长先略有下降然后上升。
It was noted that when coagulation bath temperature was increased, crystallization could be suppressed, and more porous structure was obtained on the surface of the membrane.
另外,凝胶浴温度升高可以抑制结晶现象,并使膜表面孔径和孔密度增加。
Several spinning procedure conditions were discussed, such as coagulation bath concentration, temperature, extruding rate and core layer liquid flow rate etc.
并对凝固浴浓度和温度、挤出速率、芯液流量等纺丝工艺条件进行了探讨。
The concentration and temperature of the coagulation bath and spinning conditions all have a great effect on structures and properties of PVDF/PVC hollow fiber membranes.
凝胶浴的浓度和温度、纺丝工艺等都会影响共混体系的相容性并改变膜的结构和性能。
It pointed out that the temperature of spinning solution, negative stretching, temperature of coagulation bath, concentration, flow and spin-finish had influence on quality of flat fiber.
指出原液温度、负拉伸、凝固浴温度、浓度、流量以及所用的油剂都会对扁平纤维的质量产生影响。