The annealing process was made under different temperature and holding time to the cold forging AZ31 magnesium alloy with different deformation ratio.
对不同变形量的冷锻az31镁合金在不同温度和保温时间下进行退火。
The annealing process was made under different temperature and holding time to the cold forging AZ31 magnesium alloy with different deformation ratio.
对不同变形量的冷锻az31镁合金在不同温度和保温时间下进行退火。