Simulating different solidification cooling rate with step-metal mould and sand mould, the effect of solidification cooling rate on microstructure and properties of high boron steel were studied.
利用阶梯型腔金属模和砂型模拟不同的冷却速度,研究了冷却速度对高硼钢凝固组织和性能的影响。
The influence of rare earth, titanium and nitrogen on the structures and properties of high boron alloy steel was researched.
研究了稀土-钛-氮复合变质处理对高硼合金钢组织和性能的影响。
The invention relates to chromium-tungsten-rare earth-boron series air cooling medium-high carbon bainite steel and a preparation method thereof, and belongs to the technical field of alloy steel.
本发明涉及一种铬-钨-稀土-硼系空冷中高碳贝氏体钢及其制备方法,属合金钢技 术领域。
The invention relates to chromium-tungsten-rare earth-boron series air cooling medium-high carbon bainite steel and a preparation method thereof, and belongs to the technical field of alloy steel.
本发明涉及一种铬-钨-稀土-硼系空冷中高碳贝氏体钢及其制备方法,属合金钢技 术领域。