Study shows that quenched boron eutectic structure possesses the excellent wear abrasion property.
研究表明:硼共晶组织经淬火后,具有优良的抗磨粒磨损性能。
The high chromium white cast iron was carried on wear abrasion test under different loads on the testing machine.
对不同载荷作用下的高铬铸铁在耐磨实验机上进行了磨料磨损试验;
The wear abrasion and ageing of contact is one of the important factors which affect the electromagnetic relay reliability.
电磁继电器触点的磨损和老化是影响继电器可靠性的重要因素之一。
Failure analysis of high chromium cast iron liner has been studied by the microstructure, pole-pan wear abrasion, wet grinding and impact toughness.
用微观组织分析、杆盘式磨损、湿磨法磨损和冲击韧性等试验手段,对高铬铸铁衬板的显微组织、力学性能和耐磨性进行了试验分析。
Mechanical strength, machinability, surface corrosive and wear abrasion of a new type glass ceramic composed of fluorophlgopite Ca-mice were studied in this article.
研究了一种新型的钙云母为主相高强度的可切削玻璃陶瓷的力学性能、可加工性、表面耐腐蚀性、耐磨耗性。
The ferrography, as a kind of non-disassembly fault detection and diagnosis method for wear abrasion, has been paid more attentions to the application by many experts and scholars.
铁谱技术作为一种不解体的磨损故障检测与诊断手段,已愈来愈为众多专家、学者和工程技术人员所关注。
There are over high vibrations and noises of the main steam piping lines of a Nuclear Power Plant. Wear abrasion of the main steam isolation valves was found during the fall outage.
一核电厂主蒸汽管线存在振动和噪声过大,大修时还发现主蒸汽隔离阀闸板存在一定的磨损。
For those who wear contacts which are too tight, the risks include swelling of the cornea, redness or corneal abrasion.
如果佩戴过紧的隐形眼镜,那么可能会导致使用者角膜肿胀、眼部泛红或是角膜损伤。
Dry eyes, foreign body injuries, and prolonged contact lens wear are all commonly associated circumstances for the development of a corneal abrasion.
干眼症、异物损伤、以及长时间佩戴隐形眼镜均是导致角膜擦伤发生的常见相关情况。
The pure gum rubber sleeve of the Type A Valve offers excellent abrasion resistance, and since the Type A uses only air pressure to operate, there are no moving parts to break or wear out.
型夹管阀采用的纯树脂橡胶具有优异的抗磨损能力,因为A型夹管阀只是采用气压进行操作,因此没有活动部件会断裂或磨损。
There are scouring abrasion and impact wear two basic types. The microstructure of two kinds of metal loss in process of wear and tear is not exactly the same.
有冲刷磨损和撞击磨损两种基本类型。两种磨损的金属流失过程的微观形态是不完全相同的。
Some high chromium steels can be hardened by heat treatment and are used where resistance to wear, abrasion, and corrosion are required.
一些高铬钢能通过热处理硬化,可用于抗磨坏,抗磨损,抗腐蚀需求的地方。
Polyurethane film handily outperforms many other common polymers when it comes to abrasion resistance. Five times more resistant than natural rubber, the material is of choice of wear products.
聚氨酯薄膜的耐磨性胜过许多其他常见的聚合物。较天然橡胶耐磨五倍以上,是耐磨制品的首选材料之一。
Home after entry in wear slippers, best reduce sand dust abrasion on the surface of a landscape stone.
住家最好入门后换穿拖鞋,减少砂粒尘土磨损景观石表面之机会。
It is concluded that the mechanisms include gouging abrasion and fatigue wear.
认为其机制主要是:凿削式磨粒磨损和疲劳磨损。
The wear mechanism of TO-treated alloy was slightly abrasion.
改性钛合金的磨损机制为轻微的磨粒磨损。
Pilling is often the first sign of wear due to abrasion; it causes a cloth to have an unsightly and disheveled appearance.
起球现象是服装穿着磨损的第一个信号,它使织物的外观不雅而且松散杂乱。
Grain wear and fatigue wear were the main wear styles in the process of abrasion of all surface-strengthened samples.
几种表面强化的试件与不锈钢的磨损表明,主要磨损形式为磨粒磨损和疲劳剥落。
The influence of varying impact energy on wear resistance of dual phase cast steel has been investigated under impact three body abrasion.
在动载三体磨粒磨损条件下,试验研究了冲击载荷的变化对铸态复相耐磨钢动载磨粒磨损特性的影响。
But the jaw plate must be replaced frequently because the abrasion is severe for intense impact and attrition wear from ores.
但是,由于颚式破碎机工作时受到矿石的强烈撞击和磨损,磨损仍然非常严重,几天就需要更换新的颚板。
Under three different impact energy, LCHA with Mn in place of Ni were tested with a modified MLD-10 wear tester to investigate their behavior of corrosive impact abrasion.
在改进的MLD - 10型冲击腐蚀磨损试验机上,选择三种不同的冲击功,对以锰代镍的低碳高合金钢的冲击腐蚀磨损性能进行了测试。
Aimed at the abrasion of pins, some experiments were carried out and the abrasion course was analyzed, the abrasion course of pins is the breaking-in, the abrasion wear and adhesive abrasion.
通过大量试验,分析了装载机销轴磨损的历程,表明销轴的磨损历程主要分为磨合阶段、磨粒磨损阶段和粘结磨损阶段。
The movement patterns of abrasive particles are of important influence on the wear of materials in three-body abrasion.
在三体磨料磨损中,磨粒的运动方式对金属的磨损有重要影响。
The results show that the impact energy has great influence on the corrosive impact abrasion properties and wear mechanisms of the two steels.
结果表明,冲击功对两种钢的冲击腐蚀磨损性能和机制具有很大的影响。
For those who wear contacts which are too tight, the risks include swelling of the cornea, redness or corneal abrasion.
如果佩戴过紧的隐形眼镜,那么可能会导致使用者角膜肿胀、红眼病或是角膜损伤。
LCHA with several variations of composition were tested with a modified MLD-10 wear tester to investigate their behavior under corrosive impact abrasion.
在改进的MLD - 10型冲击腐蚀磨损试验机上,对不同成分的低碳高合金钢的冲击腐蚀磨损性能进行了测试。
The abrasiOn wear of ore-accumulation drive-over hopper is an important factor restricting increasement of equipment operation rate and production capacity.
通过式漏斗的磨损是制约选矿厂设备作业率及生产能力提高的重要因素。
The main wear mode of PPS is changed from adhesive wear into abrasion wear with the addition of PTFE and kaolin nanoparticles.
PTFE和纳米高岭土的加入使PPS的主要磨损方式由粘着磨损转变为磨粒磨损。
On the base of invalidation analysis of the wear liners of the beater, the abrasion-resistant capability experiment is carried through NJ-cast iron and Ct-white iron.
在对搅拌器中衬板失效分析的基础上,对镍硬铸铁和铬系白口铸铁进行了磨料磨损试验。
The micro-scale abrasive wear behaviors of TAMZ alloy were studied using a TE66 micro-scale abrasion tester.
采用TE66试验机对新型TAMZ钛合金的微磨粒磨损行为进行了研究。
应用推荐