Optimizing continuous casting planning is one of the important ways to get high production rate and reduce the energy consuming.
编制高效的连铸生产计划在提高生产率和降低能耗方面具有十分重要的意义。
It shows that thin slab continuous casting has a greater secondary cooling intensity, a faster solidifying rate, a fine and uniform structure and less segregation than conventional slab casting.
研究表明,薄板坯的二冷强度大,凝固速度快,组织细小、均匀,其内部溶质元素的偏析程度远低于传统连铸板坯。
So, the continuous casting was improved, the qualification rate of wide plate during flaw detection was increased.
于是对浇注过程作了改进,使宽厚钢板探伤合格率提高。