粗晶lc 4合金在较低温度和较高应变速率条件下,因能产生有效的再结晶细化,而呈现出一定的超塑性。
The coarse crystalline LC4 alloy exhibit some superplasticity under lower temperature and higher strain rate, because it can create effective recrystallization refinement.
在高温下制取的wc粉,结晶完整,晶内亚结构粗大,微观应变小。
WC powders prepared at higher temperatures are characterized by complete sintering, coarse substructure and slight micro-strain.
研究指出,应变诱发再结晶对细化晶粒和提高大角度晶界分数的作用明显地影响合金的超塑性能。
It is evident that the effects of strain-induced recrystallization on grain refining and on high-angle grain boundary fraction increasing affect greatly the superplastic properties of the alloy.