...; 煅烧时间; 分段煅烧[gap=779]Key words: spinel lithium manganese oxide; solid method in room temperature; calcine time; calcine by steps...
基于8个网页-相关网页
The effects of the calcine size, leaching temperature, leaching time and solution-solid ration no the leaching rate of the sodium chromate in the chromium calcine are investigated.
结果表明,在试验的浸出条件下,铬焙砂粒度对铬浸出率的影响不显著,铬浸出率随浸出温度升高、液固比增大和浸出时间延长而增加。
The calcine temperature and lasting time were selected as technological parameter during the calcining process.
选取的参数为:煅烧温度和保温时间(煅烧时间)。