First, all factors in PVDF membrane preparation were examined and the optimal condition of membrane preparation was gotten. The content of PVDF was wt.16%, PEG was wt.8% and the coagulating bath temperature was 30℃.
本文首先对PVDF膜制备过程中几个主要影响因素进行综合考查,得到PVDF膜的最佳制备条件为PVDF含量wt.16%,PEG400含量wt.8%,凝固浴温度为30℃。
参考来源 - 纳米SiO·2,447,543篇论文数据,部分数据来源于NoteExpress
The casting solution dropwise or linearly enters a coagulating bath by oscillation of a pinhead, and forms the polymer small ball or film after coagulating and shaping.
铸膜液通过针头振荡以滴状或线状进入凝固浴中,凝固定型形成聚合物小球或膜。
The results show that spinning and fiber properties are influenced by the concentration of the solvent in the coagulating bath and the temperature of the coagulating bath.
结果表明:凝固浴中溶剂浓度对纺丝过程及纤维强度有重要影响,而凝固浴温度对纤维的影响相对较小;