From the model, the critical effect tensile stress for the initiation of hydrogen induced crack along grain boundaries has been derived.
由该模型推导出氢致沿晶裂纹萌生时的临界有效拉应力。
Presumably, it is due to their different critical values of the ratio of slip plane hardening rate to current tensile stress for shear localization.
这可能是由于它们产生剪切形变局部化的滑移面硬化率对瞬时拉伸应力的临界比值不同之故。
Presumably it is due to their different critical values of the ratio of slip plane hardening rate to current tensile stress for shear localization.
这可能是由于在不同状态时产生剪切形变局部化的滑移面硬化率对瞬时拉应力的临界比值不同之故。