The secondary hydration of high fly ash content concrete is slow at the early period and then the velocity of it gradually increase.
高掺量粉煤灰混凝土早期二次水化较为缓慢,随后二次速度逐渐加快。
Activator can enhance remarkably the activity of fly ash and accelerate secondary hydration reaction of high fly ash content concrete.
激发剂能显著提高粉煤灰的活性,加速高掺量粉煤灰二次水化反应。
This paper introduces the mix proportion of high fly ash content concrete instead of 30% cement with fly ash and some experiment results of the test examples in laboratory.
介绍了在水泥混凝土中,采用粉煤灰替代30 %水泥的高掺量粉煤灰混凝土的配合比设计,以及试件力学性能的室内实验结果。