It is discussed that adiabatic material, as well as ratio of height and width effected solidification, shrinkage cavity and shrinkage porosity.
讨论了锭模的高宽比、绝热板材质对凝固位置及缩孔疏松的影响。
Large thick-section ductile Iron housing easily produces casting defects such as shrinkage cavity, shrinkage porosity, graphite floating and spheroidizing decay.
大型厚断面球墨铸铁件在铸造过程中极易产生缩孔、缩松、石墨漂浮及球化衰退等铸造缺陷。
Batch production shows there are no shrinkage cavity and porosity in casting, and no blowholes and sand inclusions on the top surface. The yield of the casting is 81%.
经批量生产验证,铸件内无缩孔、缩松缺陷,上表面无渣孔、气孔缺陷,工艺出品率81%。