The CCTO films prepared with different preheating temperature after rapid thermal annealing treatment have the smaller dielectric loss, and the values lie in between 0.1~0.35.
不同预烧温度所制备的CCTO薄膜,经快速热退火处理后,其介电损耗值较小,基本在0.1~0.35之间。
As a thermal oxidation procedure, the annealing treatment is not only a crystallization process but also an oxidation process.
作为一道热氧化工序,退火处理不仅是一个氧化过程,而且是一个结晶过程。