When the strain is below 0.29, the average grain size decreases obviously with the increase of strain.
当应变小于0.29时,平均晶粒尺寸明显地随应变增大而减小;
Nevertheless, after the strain reaches 0.29, the average grain size decreases slowly with the increase of strain.
当应变达到0.29时,平均晶粒尺寸缓慢地随应变增大而减小。
Ultrafine-grained 2J4 hysteresis alloy processed by equal-channel angular process(ECAP), has the average grain size approximate 0.
利用等通道弯曲挤压的方法得到的晶粒平均尺寸大约为0。