In the test, the strength grade of concrete is C20 and C60, and the cementitious system contains 10%, 20%, 30% and 40% of fly ash in accord with weight.
实验中应用的混凝土的强度等级分别为C20和C60,其中粉煤灰的掺量(胶凝材料的质量分数)分别为未掺、10%、20%、30%、40%。
In the test, the strength grade of concrete is C20 and C60, and the cementitious system contains 10%, 20%, 30% and 40% of fly ash in accord with weight.
实验中应用的混凝土的强度等级分别为C20和C60,其中粉煤灰的掺量(胶凝材料的质量分数)分别为未掺、10%、20%、30%、40%。