The rheological property, extrusion property and heat stability in the processing of PVC dry blends modified by impact ACR are introduced briefly.
简单介绍了用冲击A CR改性的PVC干混料的流变、挤出和加工热稳定性能。
The impact of various process conditions on extrusion and pelletizing is studied, including the change of extrusion speed, die head temperature and screw types.
进行了各种相关工艺条件对挤出造粒的影响,包括挤出速度、模头温度及螺杆形式和定型模具对挤出成型的研究;
The rate of extrusion has a large impact on the quality of the product and should be adjusted accordingly.
挤压比率大大的影响着产品质量,因而需要相应的调整。
Hazelett strip casting process is already successfully used for producing slug for impact extrusion.
哈兹·列特铝板带连铸连轧工艺已被成功地用于铝和铝合金冲击挤压用坯料的生产。
Lustran ABS 1152 Extrusion grade of ABS (acrylonitrile butadiene styrene). Very high impact grade with superior toughness, especially for low temperature applications, and good thermoformability.
挤出级的ABS(丙烯腈丁二烯苯乙烯)。具有超强的韧性非常高品位的影响,特别是低温应用,以及良好的热成型。
The paper discusses the basic design parameters and process parameters of the extruder, and detailed analysis the impact of these parameters on the extrusion system.
本文对挤压机基本设计参数和工艺参数进行了系统论述,将这些参数对挤压系统的影响进行了详细分析。
A 35 nom. Shore d, containing non-discoloring stabilizer, plasticiser free resin for injection molding and extrusion; with low temperature impact resistance as well as excellent mechanical properties.
一位35额定值。肖尔研发,含有非脱色剂,注射成型和挤出树脂增塑剂自由;具有低温耐冲击性以及优良的力学性能。
Use these technical parameters, carry the semisolid extrusion shaping to the slurry, then test the impact ductility, rigidity and impacting grinding abrasion.
采用上述工艺参数对浆料进行半固态挤压成形,并对挤压件进行冲击韧性、硬度和冲击磨料磨损测试。
During the process of extrusion by tri-screw extruder, the combination of mixing components in tri-screw extruder has an important impact on extrusion properties.
在三螺杆挤出机的挤出工艺中,混合元件的合理组合对三螺杆挤出机的挤出性能有着重要影响。
During the process of extrusion by tri-screw extruder, the combination of mixing components in tri-screw extruder has an important impact on extrusion properties.
在三螺杆挤出机的挤出工艺中,混合元件的合理组合对三螺杆挤出机的挤出性能有着重要影响。