Low hydrogen electrode to be used for welding thick steel plate to casting and high tensile plates.
应采用低氢焊条焊接厚钢板与铸钢件和高强度板间的连接。
Measures were taken to prevent welding cold cracking such as improve welding technology by decreasing cooling speed and adopting low-hydrogen electrode, etc.
通过改进焊接工艺来降低冷却速度和采用低氢型焊条等措施来控制焊接冷裂纹的产生。
The paper introduces the high toughnesses Ultra-low hydrogen electrode (new J807CF) which matches WCF—80 steel for manual arc welding.
本文介绍了高强高韧性超低氢新J807CF焊条,其各项性能均达到国外同类产品的先进水平,是WCF—80钢的专用配套焊条。
Low hydrogen type electrode is baked out before welding, the baking temperature and duration as specified by the manufacturer.
低氢焊条在焊前应烘干,烘干温度和时间遵照厂家说明。
Low hydrogen type electrode is baked out before welding, the baking temperature and duration as specified by the manufacturer.
低氢焊条在焊前应烘干,烘干温度和时间遵照厂家说明。