• The output power is very stable after the temperature cycling and vibration test. No apparent power decrease has been observed as the device working continuously for 500 h.

    该光纤耦合模块连续工作500小时没有发现明显的功率衰减,并且输出功率经温度循环和振动冲击后具有较好的稳定性。

    youdao

  • The thermal fatigue test was performed on 316 SS to understand the crack propagation behavior underthe cycling temperature environment.

    从实用出发对316不锈钢管材进行了热循环下的裂纹扩展试验。

    youdao

  • The thermal fatigue test was performed on 316 SS to understand the crack propagation behavior underthe cycling temperature environment.

    从实用出发对316不锈钢管材进行了热循环下的裂纹扩展试验。