The optimal weight fraction is 0.1%, for under this condition, the wear scar diameter is decreased 35.6% and lubricating oil has great time-release effect.
当铜镍复合粉体的质量分数达到0.1%时,磨斑直径降低幅度最大,达35.6%,并具有很好的长效减摩性能。