由于硫酸烧渣中的铁属于强磁性矿物,采用湿式鼓筒式弱磁选机分选是较为适宜的。
Fe in the vitriol calcigenous is a high magnetism mineral, so it is feasible to separate Fe by adopting wet drum type weak magnet separator.
采用粗粒抛尾—阶段磨矿、阶段弱磁选工艺对某低品位钒钛磁铁矿进行了选铁试验研究。
Test was made on separating iron from a low grade Vanadiferous titanomagnetite ore by a process of tailing discarding at a coarser size, staged grinding and staged low intensity magnetic separation.