The results show that the annealing temperature was reduced, the annealing time was reduced and the mechanical properties were enhanced, which has remarkable energy conservation effect.
结果表明:大大降低退火温度,缩短退火时间,提高力学性能,综合节能效果显著。
In high temperature zone, as the temperature rising wood bending strength was reduced, and compression strength perpendicular to grain had gained in strength.
在高温区域,随着温度的升高,抗弯强度被明显削弱,而横纹抗压强度则得到增强。
The daily rang of temperature and humidity were reduced, and the wind velocity was weakened.
且人工雨林内温、湿度日较差最小,对风的消弱最强。